Hey Steve
Cool pictures.
Looks like braided rope, the manufacturers put in one cluster of strands
with a different color to give it a pattern... So you can tell your
sailing crew to pull on the "green fleck" rope.
As for your wire, I'd interpret picture 3 as one cluster of strands in
the braiding has bad plating and/or something nasty contaminating it,
making it corrode. Since these are new, and they aren't going to
improve with time, I'd reject them... bad batch of wire!
regards,
- Graham
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Tuesday, June 09, 2009 10:35 AM
To: [log in to unmask]
Subject: [TN] Green Junk in Wire
Good Morning!
We've just had something come-up that really has a few of us scratching
our heads around here.
To preface this; we have a mechanical assembly building where we put
cabinents and boxes together plus do some cable and harness assembly.
Yesterday one of engineers called me and said that they were seeing some
green stuff on some of the cables that we've built and said that I
should come and take a look at it. While I was walking over to the other
building it was thinking to myself; "I hope that somebody didn't get a
hold of the wrong flux or something...".
When I got there, I was really suprised at what I saw:
http://stevezeva.homestead.com/files/Green_Junk_1.jpg
http://stevezeva.homestead.com/files/Green_Junk_2.jpg
http://stevezeva.homestead.com/files/Green_Junk_3.jpg
http://stevezeva.homestead.com/files/Green_Junk_Close.jpg
The photos that you see come from a cable assembly that is about 3-feet
long, and we're seeing it on cable assemblies that are longer. The wire
in the assembly is a PTFE insulated single conductor shielded and
jacketed cable. The conductor and shield is silver plated OFHC copper.
The photos are taken from a section in the middle of the wire well away
from any area that soldering has been done. The shields of all the wires
in the bundle get soldered together at each end using a ORL0 wire solder
and flux. The green substance appears throughout the wires. In "Green
Junk 3", you can see how the green is with a group of the strands of the
braided shield and how it spirals around the wire.
It goes without saying that I'm contacting the wire manufacturer, and
I'm sending out a cable assembly for analysis. But have any of you ever
seen this before?
Steve
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|