TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 21 Apr 2008 11:06:57 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Ted Tontis <[log in to unmask]>
Subject:
From:
Ted Tontis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (92 lines)
	I just did an audit on a Metal core manufacturer on the first of the
month. If you hadn't already I would note the dielectric material as well as
the dielectric thickness. I would also suggest you detail how you want to
singulate the PCA's, punch, V-score or both.  
	As Mr. Carter mentioned talk with the board house, they can tell you
what they need and want. Most importantly ask lots of questions if you know
what you want to do and unsure how to do it they will tell you what will
work and what will not work. If you get a chance ask them to see the
process, it will give you a better understanding of how it is put together
and the obstacles they face, it is a pretty interesting process.

Ted T.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lenny Carter
Sent: Monday, April 21, 2008 10:28 AM
To: [log in to unmask]
Subject: Re: [TN] Metal core PCB

eeek.  We just ventured into metal backed pcb for thermal management and it 
was new to us as well.
On the drawing with the manufacturing notes we simply added a detail named 
"Stackup Detail".  It is essentially a small pcb cross section.  It is a 
dimensioned cross section showing drill dia and depths.  Our pcb vendor 
helped us create the detail.  After all, they are the ones who needed it, so

it made sense to ask them what they needed and how they wanted it.  They 
essentially approved it for us before we released it.
Lenny  ERG   www.ergpower.com


----- Original Message ----- 
From: "Ioan Tempea" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, April 21, 2008 11:09 AM
Subject: [TN] Metal core PCB


Dear Technos,



How should a metal core PCB be specified? I mean besides specing 1mm
thick Aluminum and 2oz Cu, what should find its place in the tech notes?



Thanks,



Ioan


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2