TECHNET Archives

September 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
David D Hillman <[log in to unmask]>
Date:
Tue, 30 Sep 1997 16:58:44 -0500
Content-type:
text/plain; charset=us-ascii
X-To:
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, David D Hillman <[log in to unmask]>
Parts/Attachments:
text/plain (31 lines)
Hi Steve, Poh, et al!

The topic of placement accuracy is ironic - I will be presenting a paper on
our just completed placement capability effort at the IPC meeting in
Arlington next week on Wednesday afternoon in the S12 session. I don't
really talk about the data in true numbers but from a methodology
standpoint I do. We followed a two step pattern: (1) conduct a sticky tape
test to understand the equipment aspects of gauge R&R for onsertion
process; (2) conduct a solder paste test to understand the process
interaction aspects of gauge R&R on the onsertion process. If you only do
#1 then you miss an important part of the test - the interaction of the
component leads being pushed on/into the solderpaste plus any reflow
characteristics. If you only do #2 then you miss out on the equipment
contribution to the gauge R&R measurement.  Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2