TECHNET Archives

April 2014

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Tue, 8 Apr 2014 08:22:46 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (52 lines)
Hi Lyon,

Was it SMOBC (Solder Mask Over Bare Copper)? Occasionally I still see
old legacy boards that call out fused tin covered by solder mask and
some (for whatever reason) just don't want to change the drawing. Of
course the tin reflows, the mask loses adhesion and starts flaking off.
But I doubt that's your problem. When I see a board like that I tell
them that we're going to have to charge them to hand solder everything,
and most (not all) will change the board to SMOBC...hehehe.

You say that there are some boards out of the same datecode that show
this while the rest of them are okay, I would say that's a material
issue. The boards that have the mask peeling off were contaminated with
something (moisture, greasy finger prints, etc) before they were masked.
I would be giving your board vendor a call...

Steve 


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of lyonyuan
Sent: Tuesday, April 8, 2014 5:42 AM
To: [log in to unmask]
Subject: [TN] solder mask peel off after Top sider reflow

Hi Team,

 

We found some PCBA boards(the same date code) with solder mask peel off
after Top side reflow. Material issue or process issue?

 

Lyon yuan

 



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2