Larry,
I am not sure about 12%. By one hand, a lot of chemistries for copper
plating produce copper arround 20% of elongation.By other hand, I still
remeber figures arround 7% as minimum.
Determination of elongation is a little bit tricky : includes thermal
treatment of the foil for recrystalisation and very carefull preparation of
the sample to avoid scraches .
Edward
Edward Szpruch
Eltek Ltd
P.O.Box 159 ; 49101 Petah Tikva Israel
Tel ++972 3 9395050 , Fax ++972 3 9309581
e-mail [log in to unmask]
> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: ג דצמבר 03 2002 23:04
> To: [log in to unmask]
> Subject: Re: [TN] via cracking
>
> Russ,
>
> I would add just one more cause. If the copper has a low elongation, less
> than 12%, it can be brittle enough to crack.
>
> Larry
> --------------------------------------------------- Technet Mail List
> provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send
> a message to [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery
> of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of previous posts
> at: http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/html/forum.htm for additional information, or contact
> Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|