All,
Let me be bold and say that the first photo incorporates an optically
clear medium on the top surface of the chip such that when photons are
emitted out the top surface. They exit the IC - into the optical
medium. Then upon encountering the air/optical medium interface they
are totally [by design/desire] reflected back into the optical medium
and thereby optically coupled into a nearby photo-receptive portion of
the IC without the requirement for a physical trace on the chip.
The second shot appears to be of a diced wafer - active circuitry and
bond pads "Up". Being a diced wafer, there are no bond wires shown,
etc.
If it were a normal 'flip-chip' all we would see is the bare silicon on
the back-side - as the 'good' side would be down.
I am still having a problem wrapping my head around these and the very
first photo, although the first one also seems to have optical qualities
about it.
Ingemar - are we going to have to shoot you if you tell us what it is?
Steve C
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, October 09, 2006 9:32 AM
To: [log in to unmask]
Subject: Re: [TN] NTC: Friday question 2
Mornin' all Ya'll!
Inge sent me two more pictures. Took me a while to post them this
morning as we lost phase "A" of our three phase power into the building
this morning. Been running around throwing breakers and stuff. Got the
power back and now everything is back to normal.
Anywho, here's Inge's pictures:
http://stevezeva.homestead.com/files/H1.jpg
http://stevezeva.homestead.com/files/PICT0012.jpg
Obviously these are pictures of some sort of Massively Parallel
Processing computer, but what? It's not a Cray...
Inge, was the very first picture some sort of liquid cooling chamber for
the core?
-Steve-
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ingemar Hernefjord
(KC/EMW)
Sent: Monday, October 09, 2006 7:01 AM
To: [log in to unmask]
Subject: Re: [TN] NTC: Friday question 2
Smaller and smarter...and not a Cray...
Inge
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Fjelstad
Sent: den 9 oktober 2006 13:18
To: [log in to unmask]
Subject: Re: [TN] NTC: Friday question 2
Hmmmm..... Must be a Cray
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|