Hi All!
After a few technical difficulties (namely AOL) I've got Gary's pictures up.
Go to: <A HREF="http://www.stevezeva.homestead.com">http://www.stevezeva.homestead.com</A> and look at High Resistance 1-4...
-Steve Gregory-
> Good morning all,
>
> We did a cross-section to a via on a board that one of our Technicians
> found to have high
> resistance. I'll have to admit - I've never seen one like this. I will be
> sending some
> crude pictures to Steve for display. There is dark discoloration around
> the barrel to
> inter-conductor interfaces.
>
> Thanks in advance, (TIA) ;^}
>
> Gary Camac
>
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------