TECHNET Archives

January 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Wed, 19 Jan 2005 17:48:40 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Roger Tingler <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Roger Tingler <[log in to unmask]>
Parts/Attachments:
text/plain (34 lines)
Goodmorning,
Does anybody know where this different profile data was developed and by
who?
Thermal Shock Requirements: MIL-P-55110F A1, paragraph 4.8.6.2.a and Table
A-V specifies different temperature profiles for different materials. For
example, GY material has a thermal shock profile is between -40C and 85C
while the profile for GI is -65C to 170C. Each material type is tested to
100 such cycles.
Note: History: MIL-P-55110 D (1985) per paragraph 4.8.6.3 had the profile
for GY material between -65C and 150C and -65C and 170C for GI. Therefore,
some group must have added more data for different materials between
Revision D and F.

Thanks,

Roger Tingler
Methods Engineer
Colonial Circuits
V:800-578-9602 x102
   540-752-5511x102
F:800-631-0856
   540-752-4832
E-mail: [log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2