TECHNET Archives

April 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Nutting, Phil" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Nutting, Phil
Date:
Fri, 22 Apr 2016 18:29:17 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (43 lines)
Ioan,

My observation has been that wires tinned and then connected via a compression screw seem to suffer from "cold flow".  I can't say that this was the cause of failures, but I consider it a cause for concern and possibly a design improvement by using a different termination method.

My 2 cents.

Phil

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Friday, April 22, 2016 1:43 PM
To: [log in to unmask]
Subject: [TN] Compression and solder creep

Dear Technos,

Keeping solder joints under constant load decreases their life. I was reading through the chapter dedicated to creep in Klein-Wassink, but he is not specific if the type of load has an effect or simply any type of load is equally detrimental.

More specifically, is compressive load a creep accelerator, or not? E.g. keeping a weight on mated connectors, to prevent them from de-mating in vibration, would reduce the life of the solder joints of those connectors?

Thanks,

Ioan Tempea, P. Eng.
Manufacturing Engineer, Satellite Systems

[cid:[log in to unmask]]

MacDonald, Dettwiler and Associates Corporation, 21025 Trans-Canada Highway, Ste-Anne-de-Bellevue, QC, Canada H9X 3R2
Tel: +1-514-457-2150 x3556
www.mdacorporation.com<http://www.mdacorporation.com/>

This e-mail, and any attachments, are intended solely for the use of the intended recipient(s) and may contain legally privileged, proprietary and/or confidential information. Any use, disclosure, dissemination, distribution or copying of this e-mail and any attachments for any purposes that have not been specifically authorized by the sender is strictly prohibited. If you are not the intended recipient, please immediately notify the sender by reply e-mail and permanently delete all copies and attachments. This email is for informational purposes only and shall not be interpreted to authorize or conclude a binding agreement between MDA and any other party unless this email contains or is accompanied by an express written confirmation of MDA's intention to enter into a binding agreement, such confirmation shall only be provided by an authorized representative of MDA.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2