TECHNET Archives

October 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 21 Oct 2010 15:05:53 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Werner Engelmaier <[log in to unmask]>
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Content-Type:
text/plain; charset="utf-8"
In-Reply-To:
<FA906DF27A4A418B9A66F6C5A71B5FAE@BobWork>
Content-Transfer-Encoding:
quoted-printable
MIME-Version:
1.0
Parts/Attachments:
text/plain (145 lines)
 Hi Bob,
With your application you want to have a Tg of at least 150C—you need to remember that glass transition is a process that takes place over about a 50C temperature range; so for Tg=150 it starts at about 125C. 
The biggest issue most likely will relate to barrel fractures.

 
 
Werner
Upcoming workshops:
November 2 & 9, SMTA Webtorial,
     “Fundamentals in Solder Joint Reliability”
December 7 & 14, SMTA Webtorial,
     “Acceleration Models, Accelerated Reliability Tests and ScreeningProcedures”


 

 

-----Original Message-----
From: Robert Kondner <[log in to unmask]>
To: [log in to unmask]
Sent: Thu, Oct 21, 2010 1:12 pm
Subject: [TN] FR4 Temperature and Life


Hi,



 



 I was looking around and I found some references to "FR4" as having a Tg

from 100 to 130 C. I was surprised as I thought that seemed low.



 



 Now I understand that FR4 is a pretty wide brush and it covers a lot of

different materials and different suppliers.  BUT, I was wondering what

"Most" PCB vendors are supplying and how the Tg affect life with hot

components.



 



 I have some small QFN parts that tend to run hot, PCB temps of 100C or a

little more. Forgetting thermal cycling for a moment does a 100 to 120 C

temperature induce failures in other area like copper foil to base

separation, de-lamination, solder interface or any other failure mode?



 



 Any pointers to literature?



 



Thanks,



Bob K.







______________________________________________________________________

This email has been scanned by the MessageLabs Email Security System.

For more information please contact helpdesk at x2960 or [log in to unmask] 

______________________________________________________________________



---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 15.0

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to 

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to 

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 

additional information, or contact Keach Sasamori at [log in to unmask] or 

847-615-7100 ext.2815

-----------------------------------------------------


 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2