TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Lee parker <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Lee parker <[log in to unmask]>
Date:
Tue, 20 Sep 2005 22:31:00 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (47 lines)
Michel

Those who are familiar with Auger will tell you it is the method of choice for surface analysis. It only penetrates angstroms into the surface and you can sputter a controlled depth into the surface. The only issue I have ever encountered is the operator; you need an expert to operate the machine and interpret the results.

Best regards

Lee

J. Lee Parker, Ph.D.
JLP Consultants LLC
804 779 3389 
  ----- Original Message ----- 
  From: Arbour, Michel<mailto:[log in to unmask]> 
  To: [log in to unmask]<mailto:[log in to unmask]> 
  Sent: Tuesday, September 20, 2005 5:11 PM
  Subject: [TN] ENIG contaminant : Auger analysis recommended ?


  Hi
  We will be sending non solderable PCB for analysis. Goal is to detect black
  nickel, black pad, soldermask contamination before plating or other
  contaminant. Is Auger analysis with ion sputtering (SAM) an effective method
  to determine the contaminants. Is this method proven and accepted in the PCB
  industry for this task ?

  Michel Arbour

  ---------------------------------------------------
  Technet Mail List provided as a service by IPC using LISTSERV 1.8e
  To unsubscribe, send a message to [log in to unmask]<mailto:[log in to unmask]> with following text in
  the BODY (NOT the subject field): SIGNOFF Technet
  To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet NOMAIL or (MAIL)
  To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]<mailto:[log in to unmask]>: SET Technet Digest
  Search the archives of previous posts at: http://listserv.ipc.org/archives<http://listserv.ipc.org/archives>
  Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16<http://www.ipc.org/contentpage.asp?Pageid=4.3.16> for additional information, or contact Keach Sasamori at [log in to unmask]<mailto:[log in to unmask]> or 847-615-7100 ext.2815
  -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2