TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"David D. Hillman" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 13 May 2009 13:58:00 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (72 lines)
Hi Genny - Nylon is the generic name for a family of Polyamide polymers 
first introduced in the US by Du Point (extra bonus points if someone can 
tell me what year!). Do you have the specific tradename of the nylon you 
are dealing with (e.g. Zytel, Rilsan)? Or get a copy of the Handbook of 
Electrical and Electronic Insulating Materials,  W. Tillar Shugg, ISBN 
0-7803-1030-6 which has an excellent chapter on nylon material properties. 
Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




Genny Gibbard <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
05/13/2009 01:43 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Genny Gibbard <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Nylon connectors - moisture sensitivity






We have been told that a surface mount nylon connector we use is
moisture sensitive, and should be treated as equivalent to level 5a.
This is the highest level we have ever seen on any component we have
used of any type.  I didn't think that a connector could be moisture
sensitive.  Not heat tolerant, yes - we have melted a few - but moisture
sensitive? 
What kind of damage can happen to a nylon connector from too much
moisture absorption?
Thanks in advance for your responses.

Genny 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2