Come on, guys! All "I" said was the launch failure was due to a "Bad
solderjoint". I never said anything about the actual mechanism, what
type component, leadfinish or any other metric and/or
mechanism---because I don't know. All I want is the "best joint
possible" for any product type. That means getting good,wetted
side/heel fillets for all leaded SMT devices.
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: Tuesday, June 30, 1998 3:07 PM
To: [log in to unmask]; [log in to unmask]; [log in to unmask]
Cc: [log in to unmask]; [log in to unmask]; [log in to unmask];
[log in to unmask]
Subject: Re: Pramod Patel/solder joint reliability
Hi Mark & Vern,
It definitely is news to me, "that the China Launch problems were due to
a lack of side/toe filleting". Failure at launch can only mean one of
two
things: (1) the solder joint was never properly made (wetted), or (2)
inappropriate flight-hardware testing prior to launch accummulated too
much
fatigue damage (micro/macro-cracks) to withstand the mechanical loads
during
launch (see Hubble, Magellan, Gallileo). In neither case, would the
presence
of side/toe filleting made a signficant difference.
Side fillets will defintely increase the peeling stress required due to
the
forces necessary to rip through them; that does not however equate to a
more
reliable solder joint in the long-term. If you have inadequately wetted
solder
joints, however, solder and toe fillets will likely prolong the time at
which
an infant mortality failure will occur in the short-term.
The decision makers for "Missile, Launch Vehicle, wartime avionics/sonar
and/or Spacecraft" should properly educate themselves as to what and
what not
solder joints can do. #1 issue: get away from large ceramic components
on
FR-4, #2 issue: qual testing should not be done on flight-hardware.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask]
In a message dated 6/30/98 10:38:55, [log in to unmask] wrote:
>I suggest you fellas do some more homework before drawing to Mark's
>conclusion, as one "can always make the statement that proper wetting
>makes for better peel strengths", independent of which surfaces you are
>discussing. Side fillets(PROPERLY wetted) make a VERY SIGNIFICANT
>difference in peel strengths of properly formed gull-wing and/or J-Lead
>products. The issue is not the raw peel strength itself, but the
>long-term reliability of the joints continuously under
thermo-mechanical
>stress. That is where the side-fillets become essential to long-term
>reliability of our systems.
>
>Bottomline, do YOU want to be responsible for Missile, Launch Vehicle,
>wartime avionics/sonar and/or Spacecraft failures due to simple
>solderjoint issues??
>
>I firmly believe you all are playing with fire in downplaying the
>importance of "side-fillets" to long-term solderjoint reliability.
>
>You likely missed or ignored the "multi-millions" lost on the China
>launch due to a simple solderjoint failure(??)
>
>----Original Message-----
>From: Kwoka, Mark [mailto:[log in to unmask]]
>Sent: Tuesday, June 30, 1998 10:47 AM
>To: [log in to unmask]
>Cc: [log in to unmask]; [log in to unmask];
>[log in to unmask]; [log in to unmask]; [log in to unmask]; Kwoka,
>Mark
>Subject: RE: RE: Need Pramod Patel's email address and/or telephone #
>
> Werner,
> Thanks for the clarification. Your second and fifth points are what I
was
>after. I infer that if inadequate wetting of the lead to the board
> land is infact present, then the "lead peeling test" will indicate
lower
>"peeling forces" than would be obtained from identical leads
> that were "adequately wetted". Also, side fillets are not important
if
>adequate lead wetting is exhibited.
> Regards,
> Mark
> -----Original Message-----
> From: [log in to unmask] [SMTP:[log in to unmask]]
> Sent: Wednesday, June 17, 1998 4:33 PM
> To: Kwoka, Mark
> Cc: [log in to unmask]; [log in to unmask];
>[log in to unmask]; [log in to unmask]; [log in to unmask]
> Subject: Re: RE: Need Pramod Patel's email address and/or
>telephone #
>
> Hi Mark,
> First, there is no such thing as a 'lead pull test;' while you
are of course
> pulling on the lead, what you are doing to the solder joint is
peeling it-
the
> proper reference is a lead peeling test. Some of your notions
about solder
> joint strength result directly from the false mental picture
resulting from
> the words 'tensile pull'.
> Second, the solder joint strength, as determined by a lead
peeling test, has
> no bearing on the reliabilty of the solder joint, provided the
peeling test
> does not reveal inadequate wetting.
> Third, in a peeling test you always need to observe the whole
peel-load
> history for the whole peeling process; with a 1T or larger heel
fillet, the
> largest load will be at the initial portion of peeling through
the heel
> fillet, with lower loads subsequently depending on whether or
not (at to
what
> extent) side fillets are present.
> Fourth, the fracture surface of the peeled solder joints give
typically more
> infrmation than do the peel-load histories, because the ONLY
realy important
> finding is whether or not adequate wetting has taken place.
> Fifth, the reliability in actual use does to a large extent
depend on the
heel
> fillet and the 'bottom flat' wetting; if the foot length is <3W,
than also
on
> the presence of a toe fillet, because short feet 'rock' during
thermal
> cycling. Side fillets are less important, unless you have
wetting problems.
>
> Werner Engelmaier
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|