TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Guy Ramsey <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Date:
Thu, 9 May 2013 08:32:52 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (36 lines)
Gold dissolves into the solder. Then, when you remove the solder you also
remove the gold. 
A simple analogy is like sugar in water. Imagine a cup with sugar stuck to
the inside. Fill it with hot water. Sugar dissolves, pour out hot water,
sugar goes with it. 



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert DeQuattro
Sent: Thursday, May 09, 2013 8:28 AM
To: [log in to unmask]
Subject: [TN] Gold Removal

Hello Fellow Technetter's,

I have a question on J-Std-001E 4.5.1 Gold removal which states a double
tinning process  or dynamic solder wave may be used.  Can any of you
describe this process.  How is the gold actually removed?  Or is it just
being tinned?  Gold melts at over 1000 C so I am a little confused.

Thanks,

Bob

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2