When ever there is a significant difference between the SM-782 and the
manufacturer's suggested pad; doubt the manufacturer. I know your pain.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Ken Carlile
> Sent: Friday, July 26, 2002 2:58 PM
> To: [log in to unmask]
> Subject: [TN] Help make a difference
>
>
> There has been recent discussion on whose footprint to use
> when laying out a PCB. We opted to use the manufacturers
> since it was an RF application and IPC’s was much larger then
> the designer wanted. It just so happened that the
> manufacturers data sheet contained a typo. This problem was
> not discovered until after the first production run of boards.
>
> This mistake cost our company quite a bit of money:
>
> $2,500 rework charge
> $2,455 Cost to replace the bare boards already ordered
> $2,500 Engineering cost to redesign the PCB layout
> ======
> $7,455 Total
>
> The manufacturer only agreed to pay $2,955 (the $2455 to
> replace boards plus $500 for rework).
>
> $7,455 Total
> $2,955 Settlement
> ======
> $4,500 Lost by our company!
>
> Vishay is a large company and I feel they need to be more
> accountable for their mistakes. Our company accepted the
> settlement, but I am still not pleased. If this happened to
> me it could happen to you!!! Please take a minute to email
> Dale and let them know that we as the consumer are not happy.
> You can make a difference and bring the industry back to the
> great business it used to be.
>
> Coincidently, after we notified them of this error, they
> added legal statements to their documentation freeing them
> from liability caused by any misinformation. So if and when
> it happens to you, they won't be liable!!!
>
> Please address your emails to:
> [log in to unmask]
>
> Thanks in advance for your support!
>
> --------------------------------------------------------------
> -------------------
> Technet Mail List provided as a free service by IPC using
> LISTSERV 1.8e To unsubscribe, send a message to
> [log in to unmask] with following text in the BODY (NOT the
> subject field): SIGNOFF Technet To temporarily halt or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE
> mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest Search the archives of
> previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/html/forum.htm for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-509-9700 ext.5315
> --------------------------------------------------------------
> -------------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|