TECHNET Archives

February 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 10 Feb 2006 14:02:07 -0800
MIME-version:
1.0
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Peter Lee <[log in to unmask]>
Content-type:
text/plain; charset=us-ascii
Subject:
From:
Peter Lee <[log in to unmask]>
Content-disposition:
inline
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (23 lines)
Technet,

Has anyone experienced the metal film being being washed off during in-line clean(with saponifier)? The film would come off after wash at the locations near the end of the barrel. The resistor band would still reman visible.

Would there be any impact to the form/fit/function of the component with a partially stripped coating?

Here's a link to the manuf site for the power resistor.
http://www.phoenixpassives.com/resistors/power_resistor_pr01_pr02_pr03.pdf


Rgds,
Peter

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2