TECHNET Archives

May 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain; charset="US-ASCII"
Sender:
Subject:
From:
Bill Kasprzak <[log in to unmask]>
Date:
Fri, 20 May 2005 10:25:00 -0400
MIME-Version:
1.0
X-To:
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (38 lines)
Morning Technetters,

I thought I would try to get this in before the Friday Follies (NTC)
begins.

I have a board that we have wave soldered and I have a number of joints
where the solder reaches the top side pad then stops as if though there
was a barrier. Upon closer examination, I noticed that there is something
not quite right near the edge of the  hole on the top side. I remember
reading about "Knee" problems on PTH's on this forum and searched the IPC
archives for more information. I couldn't find anything.

So I'm asking the community at large to comment about this condition at
the "knee" and the causes for it. We are certainly able to do touch up on
these joints but I'd like to try and see this before we process the board.
There are a couple of pictures that Steve G has graciously placed on his
"Picturepallooza" site.

Go to: http://www.stevezeva.homestead.com

The picture names are, "Topside Fillet and Topside Fillet 2".

Let me know what you think. Thanks.

Bill Kasprzak
Moog Inc

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Process Engineer, Electronic Assembly

ATOM RSS1 RSS2