Bill,
How many components are you soldering on each board. If it is only a
couple, I would agree with Steve Gregory that a Zephyrtronics system is
a good alternative process to the Airvac. If you have a board full of
connectors we might have a system that could help you out.
We ran .188" boards here for a customer and were getting good hole fill.
I have talked to them since and they have been using the system
successfully on boards up to .250". This machine runs a slow process
with lots of preheat so its not really suitable for high volume but does
a good job on thick boards. If you would like more information please
give me a call.
Steve Pence
Unit Design, Inc.
714-672-9944
Mengers, William D. wrote:
>Hi everyone,
>
>I am a Manufacturing Engineering in an area that builds test equipment for
>airborne radar systems. For the past several months Design Engineering has
>been giving us a variety of "thick" boards to which to solder thru hole
>components. The boards range in thickness up to .250". We have been
>substituting press-in sockets where possible, but they are not always
>available in the sizes we need. So far, in the most difficult situations, I
>have been using an Airvac solder volcano. This works fairly well, but can't
>be used in all situations, and doesn't always result in flow thru to the
>other side.
>
>Is there any other system that would be more appropriate for thick boards
>where flow thru is a problem? We are working to J-Std-001B Class
>3. We are ready to go back to the designers (and have gone back to them),
>but I would like to find out if there are other possibilities first.
>
>Thanks for any help you can give,
>
>Bill Mengers
>Mfg. Engineer
>Northrop Grumman Corp.
>Baltimore
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
>-----------------------------------------------------
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|