TECHNET Archives

August 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Date:
Wed, 17 Aug 2005 14:52:13 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
From:
Bev Christian <[log in to unmask]>
X-cc:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (42 lines)
I am sending this message with the explicit blessing of IPC staff.

The Electrochemical Migration Task Group has a time of Wednesday,
October 26th, 8 AM - 12 Noon booked for a meeting at IPC Works.  The
committee has published the CAF Test Method; the Guide to go along with
it is complete; the latter has been voted on; accepted and is in the
long, long queue to be published.  It may or not see the light of day
before IPC Works.

The Co-Chairs, Karl Sauter and myself, are soliciting presentations on
electrochemical migration or CAF - the former if someone wants to make a
pitch for a new ECM test, the latter if someone wants to champion a new
test board or has significant data to present on method or materials
that they would like to bounce off the committee before you go whole-hog
and write it up as a paper. If there are no takers, we see no reason to
hold a meeting this fall for this committee and will instruct the IPC to
delete the scheduled meeting from the program.

You can respond to me or to one of the other two gentlemen listed in the
cc above.  Thank you for your consideration.
Regards,
Bev Christian, PhD, Manager,
Materials Interconnect Lab
Research In Motion
Co-Chair, Electrochemical Migration Task Group




---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2