TECHNET Archives

March 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Thu, 5 Mar 2015 20:51:14 -0500
Reply-To:
Message-ID:
<016a01d057b0$07b38310$171a8930$@com>
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="us-ascii"
Organization:
R&D Interconnect Solutions.com
MIME-Version:
1.0
Parts/Attachments:
text/plain (16 lines)
Can anyone give me a nutshell difference between immersion tin for a solder
finish and electroplated tin? 
Advantages, disadvantages as a surface finish more than the chemical and
plating process differences. 
Thanks,
Guy





______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2