Hi Keith,
Can you post the link to his site. I would like to look at the pics for
review. Crack vias will come from the copper plating baths.
Highest Regards,
William W. DeCray III
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Keith Calhoun
Sent: Friday, April 18, 2003 2:25 PM
To: [log in to unmask]
Subject: [TN] Cracking in vias
We have recently found a problem in several assembled boards which failed
ICT. We found several vias which had become opens after
assembly. We had the open vias sectioned, I sent Steve Z. some pictures to
post on his site. I would like to have your opinions on what may
have been the cause for this failure. So far it seems to have occured only
on boards having two date codes from our board vendor.
Thanks for the support.
Keith Calhoun
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|