TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 9 Jul 2008 16:31:36 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Franklin D Asbell <[log in to unmask]>
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (52 lines)
You don't need additional coupons to tell you it is not aligned. The whole
panel is a coupon when you view the cores after inner-layer imaging, I could
never understand why they would add "more coupons" to tell you what your
eyes or AOI will tell you when inspecting the usable image. Just put the
core layers on a light table and in 5 seconds you can tell if it is
registered, in what orientation any mis-registration might be, etc. 

Just look at your A or B coupons, if you see quarter moon shaped images
where the pads do not align correctly, there is your shifting..... just my
opinion of course.

Franklin

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ted Tontis
Sent: Wednesday, July 09, 2008 4:08 PM
To: [log in to unmask]
Subject: Re: [TN] PCB Inner layer shifting

5) How would you know if you have inner layer shifting? 

Take a look at IPC 2221A, table 12-1 and figure 12-14 show registration
coupons that could be used.

http://members.ipc.org/committee/drafts/7-11_d_Coupons.pdf

Ted T 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2