TECHNET Archives

November 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Graham Naisbitt <[log in to unmask]>
Date:
Thu, 27 Nov 1997 11:35:56 UT
X-cc:
Nicholas Kane <[log in to unmask]>
Reply-To:
"TechNet Mail Forum." <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Parts/Attachments:
text/plain (101 lines)
Nicholas,

It is Residual Organic Solvent Extraction testing. Otherwise known as SEC
Solvent Extraction Conductivity or IONIC EXTRACT CLEANLINESS testing.

I am sure you will be familiar with this test method but please bear in mind
that it will only identify ionic residues that may be harmful but not any
non-ionic residues which may also be harmful. Furthermore, it is of
questionable use if you are operating a no-clean process because many fluxes
should not be cleaned and this test method does exactly that.

The method used may also impart different "cleanliness" values and you need to
apply the equivalency factor for the system used. Also, high pressure spray
systems, such as our ICOM series, provide superior extraction to those relying
on immersion.

You may also consider that the "cleanliness" value, presently recommended at
less than 1.5 microgrammes of sodium chloride equivalence, also means that it
is acceptable to leave UP TO that amount on every square centimeter of your
assembly! If you manufacture fine pitch, BGA, COB and other "exotic" chip
scale packaging, then this value will almost certainly prove too high.

For the above reasons, Surface Insulation Resistance (SIR) testing is becoming
far more relevant and if you would like some further info on that - because
guess what; we do those too - then let me know.

Sorry to give you such an extended reply, but the Americans are on holiday -
for some reason, we British aren't too sure why! - and my e-mail cupboard was
not very full.

Graham Naisbitt


Concoat Ltd                                     Email: [log in to unmask]
Alasan House, Albany Park                       Tel:    +44 (0)1276 691100
Camberley, Surrey GU15 2PL UK           Fax:    +44 (0)1276 691227


-----Original Message-----
From:   TechNet  On Behalf Of Nicholas Kane
Sent:   Monday, November 17, 1997 10:55 AM
To:     [log in to unmask]
Subject:        Re: [TN] Do we really need ionic contamination measurement
  equipment?

Please, can you tell me what ROSE is?
Thankyou
At 09:53 15/11/97 UT, you wrote:
>Ken,
>
>Your wash system is tracking the resistivity or conductivity of your rinse
>water and your filter plant is taking care of such contaminants that are
>entering the process.
>
>The question is how much contamination is on the assembly, and has it all
been
>removed? I doubt that you can accurately maintain the amount of contamination
>that is being applied to your assembly both in your process and that of your
>PC Fab shop.
>
>It is therefore a good idea to conduct regular ROSE tests to ensure that your
>process is always under control. The sampling rate to achieve that is another
>subject that should be addressed.
>
>Graham
Naisbitt>---------------------------------------------------------------------
------
>

Nicholas Kane
Axion Australasia
Suite 3, 651 Canterbury Road
Surrey Hills
Victoria 3127 Australia

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2