TECHNET Archives

July 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Jose Marroquin <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Jose Marroquin <[log in to unmask]>
Date:
Wed, 5 Jul 2006 10:37:06 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (55 lines)
All,

Recently we clean up residue on some boards with multipurpose Mr. Clean.

Should I expect problems from it?

Thanks.


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Susan Mansilla
Sent: Wednesday, January 04, 2006 5:16 PM
To: [log in to unmask]
Subject: Re: [TN] Rocha Laminate Voids..

If they are in the prepreg and are present as pressed, then there is a
mismatch between the prepreg and pressing conditions.  Are you able to do a
flow
test on some sheets of prepreg alone to see if the % flow is as  expected?
Can
you determine if you are getting the predicted thickness of  the prepreg
layer?  Are you able to determine if you are hitting the  correct temp
before you
hit the higher pressure during the lamination  cycle?

Is the excess around the edges of the panel "frothy" in appearance?

Just little thoughts that I would use to attack and "fix" the  problem.

Susan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2