TECHNET Archives

August 2000

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Roger M. Stoops" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Tue, 1 Aug 2000 14:29:12 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (103 lines)
Steve-o,

I've never used the GXT parts before,  but I remember when Berg/DuPont/FCI
came out with the GXT plating in response to the extremely high Gold prices
at the time (around 1983/4 I think, no kid, no mortgage, no gray hair...).
Gold actually got up to around $800 an OUNCE.  Connector suppliers were
adding surcharges or adders to make up the difference in cost.  This
actually spurred some changes in the connector industry, when manufacturers
then came out with "selective Gold" plating to use less gold and still
provide a solderable product (typically nickel plated part w/gold on
contact area and tin or tin/lead plating on solder tail).

I'm sure there are some other 'Netters that can add a little more to this,
and they can let me know if I got it right.  It's been so long ago.. ;-)

p.s.: my daughter is a cute kid...

Roger M. Stoops, C.I.D., PCB Designer


Spectra Precision Inc./Trimble Navigation Ltd.
5475 Kellenburger Rd.
Dayton, OH 45424-1099 USA
Ph: 937.233.8921 or 937.233.4574 ext 288
Fax: 937.233.7511


                                                                                                      
                    "Stephen R.                                                                       
                    Gregory"             To:     [log in to unmask]                                      
                    <SteveZeva@AO        cc:                                                          
                    L.COM>               Subject:     [TN] Connector Pre-tinning (don't have to!)     
                    Sent by:                                                                          
                    TechNet                                                                           
                    <[log in to unmask]                                                                     
                    ORG>                                                                              
                                                                                                      
                                                                                                      
                    08/01/00                                                                          
                    01:43 PM                                                                          
                    Please                                                                            
                    respond to                                                                        
                    "TechNet                                                                          
                    E-Mail                                                                            
                    Forum.";                                                                          
                    Please                                                                            
                    respond to                                                                        
                    SteveZeva                                                                         
                                                                                                      
                                                                                                      



Hi ya'll!

I just got off the phone with a gentleman from FCI...the plating that is on

the connectors I was talking about yesterday is something they call GXT?,
which is actually palladium nickel alloy with gold flash. I was told by FCI

that it wasn't necessary to pre-tin the connectors, that there wasn't
enough
gold on the pins to worry about...

Not that I don't trust them, but do any of you know more about this GXT?
plating? Just trying to learn more...

Thanks!

-Steve Gregory-

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################



##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2