TECHNET Archives

April 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stadem, Richard D.
Date:
Mon, 30 Apr 2012 14:56:17 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (75 lines)
Steve, 
Somewhat related to the other discussion on cleaning of no-clean:
Do you wash the assemblies after reflow, and is that why you do not see any mid-chip solder balls?
Do you wash any CCAs that have been processed with a no-clean solder paste or no-clean wire solder?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, April 30, 2012 2:42 PM
To: [log in to unmask]
Subject: Re: [TN] Homeplates on 4 mil thick stencils?

BTW I forgot to add I don't homeplate anything...

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Monday, April 30, 2012 3:16 PM
To: [log in to unmask]
Subject: Re: [TN] Homeplates on 4 mil thick stencils?

Hi Ioan,

We use 4-mil thick stencils quite often and I don't see mid-chip balling...

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: Monday, April 30, 2012 2:54 PM
To: [log in to unmask]
Subject: [TN] Homeplates on 4 mil thick stencils?

Dear Technos,

 

It is my first 4 mil stencil and I was wondering if mid-chip balling is still an issue at this thickness (no-clean process). Should I still homeplate the apertures of passives, as I fear insufficient solder?

 

Thanks,

 

Ioan Tempea, ing.
Ingénieur Principal de Fabrication / Senior Manufacturing Engineer T |
450.967.7100 ext.244 E | [log in to unmask] <mailto:[log in to unmask]> W | www.digico.cc <http://www.digico.cc/> 

 
 N'imprimer que si nécessaire - Print only if you must

 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2