Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Chuck Brummer <[log in to unmask]>
Date:
Mon, 19 Dec 2016 15:08:00 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
Parts/Attachments:
text/plain (53 lines)
There is more than one "black pad".

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Chuck Brummer
Sent: Friday, December 16, 2016 9:57 AM
To: [log in to unmask]
Subject: Re: [TN] Black Oxide issues with ENIG plating

I think you mean black pad.



Chuck Brummer
Medical Flex, EMSD
8357 Canoga Ave, Canoga Park, CA 91304-2605
Office: +1 818 734-4930 | Mobile: +1 805 890-8452 [log in to unmask]



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Lehmicke, Michael
Sent: Thursday, December 15, 2016 5:54 PM
To: [log in to unmask]
Subject: [EXTERNAL] [TN] Black Oxide issues with ENIG plating

What is the root cause of Black Oxide issues in ENIG plating?

Mike Lehmicke
Project Engineer
DSS Division
Molex, LLC-Printed Circuit Solutions
22 Empire Drive
St. Paul, MN 55103
651-846-7728
[log in to unmask]<mailto:[log in to unmask]>

[cid:[log in to unmask]][cid:[log in to unmask]]<http://www.molex.com/>


________________________________



CONFIDENTIALITY NOTICE: This message (including any attachments) may contain Molex confidential information, protected by law. If this message is confidential, forwarding it to individuals, other than those with a need to know, without the permission of the sender, is prohibited.

This message is also intended for a specific individual. If you are not the intended recipient, you should delete this message and are hereby notified that any disclosure, copying, or distribution of this message or taking of any action based upon it, is strictly prohibited.

English | Chinese | Japanese
www.molex.com/confidentiality.html
3M security scanners have not detected any malicious content in this message.

To report this email as SPAM, please forward it to [log in to unmask]

ATOM RSS1 RSS2