TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
Old-Return-Path:
Date:
Fri, 17 Jan 1997 10:43:08 GMT-0500
Precedence:
list
Reply-To:
Resent-Sender:
TechNet-request [log in to unmask]
Content-Transfer-Encoding:
7BIT
Status:
O
Priority:
normal
X-Status:
X-Loop:
TO:
[log in to unmask] (Mitch Morey)
X-Mailing-List:
<[log in to unmask]> archive/latest/9355
Return-Path:
<TechNet-request>
Resent-From:
Resent-Message-ID:
<"EsHfi.0.9DM.mrvto"@ipc>
content-length:
2379
X-Mailer:
Pegasus Mail for Win32 (v2.42a)
From [log in to unmask] Fri Jan 17 16:
39:08 1997
Subject:
From:
"Jeff Neisess" <[log in to unmask]>
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vlGPB-0000TsC; Fri, 17 Jan 97 09:40 CST
Cc:
Organization:
Eurotherm Controls Inc
Message-Id:
Parts/Attachments:
text/plain (53 lines)
> Date:          Thu, 16 Jan 1997 15:22:22 -0800
> From:          [log in to unmask] (Mitch Morey)
> To:            [log in to unmask]
> Subject:       RE: Design issues (current carrying variables)
> Cc:            [log in to unmask]

> To anyone who might be able to help,
> 
> I'm working with an engineer who is determining necessary copper widths of
> voltage nets, and he has come across some electrical properties of 1/2 oz and
> 1 oz CU that he has asked me to verify. Does anyone know wher one might possess
> such a thing (say an IPC spec?)?
> 
> I would appreciate any and ALL material properties anyone can provide.
> 
> Thanks in advance.
> 
> Mitch Morey
> [log in to unmask]
> (610)450-0994 x-17
> 
> ***************************************************************************
> *   The mail list is provided as a service by IPC using SmartList v3.05   *
> ***************************************************************************
> * To unsubscribe from this list at any time, send a message to:           *
> * [log in to unmask] with <subject: unsubscribe> and no text.*
> ***************************************************************************
> * If you are having a problem with the DesignerCouncil, please contact    *
> * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
> ***************************************************************************
> 
IPC-D-275 pages 9-11 discuss conductor width/spacing in relation to 
current capability at specific temperatures.  Hope this helps.

Jeff 
 
Jeff Neisess            EMAIL [log in to unmask]
Eurotherm Controls, Inc
11485 Sunset Hills Rd.
Reston, VA 20190  USA

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2