Lenny, et al:
Thanks for the info.
Joe Hurst
> -----Original Message-----
> From: Lenny Kurup [SMTP:[log in to unmask]]
> Sent: Friday, May 08, 1998 1:42 PM
> To: Hurst, Joe
> Subject: Re: [TN] Fr4 material
>
> Hello Joe,
>
>
> The products of combustion of the tetrafunctional, FR-4, laminate are
> as
> follows:
>
>
> carbon monoxide, carbon dioxide and bromine gas.
>
>
> Hope this information is helpfull.
>
>
> Regards,
> Lenny Kurup
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|