TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Fri, 29 Nov 1996 21:09:09 +0500
Precedence:
list
Resent-From:
From [log in to unmask] Tue Dec 3 14:
38:13 1996
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/8088
X-Sender:
[log in to unmask] (Unverified)
TO:
Return-Path:
<TechNet-request>
X-Loop:
Resent-Message-ID:
<"sA9fI1.0.U9I.L1mdo"@ipc>
Subject:
X-Priority:
1 (Highest)
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vTUoQ-0000R6C; Fri, 29 Nov 96 09:25 CST
From:
X-Mailer:
Windows Eudora Light Version 1.5.4 (16)
Message-Id:
Parts/Attachments:
text/plain (23 lines)
we find blowholes in entek finished pwbs.these are in bga pth holes. (finish 
dia 0.25 m.m) The coating thickness within specs (0.25 to 0.45). no blow
holes in other leaded components.

solder float tests done after entek with rma flux indicate good
solderability with NO BLOWHOLES (235 deg C) on bga holes.

the assembly process is apply solder paste, mount component and pass through IR
reflow.solder paste is screen printed on on bga holes also.

can somebody throw more info on above problem

thanks in advance

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2