I wouldn't. That is the last thing I would recommend. But it depends on
the use environment.
QFNs already have major issues with solder joint cracking due to CTE
mismatch. It is more likely you will have SJ reliability issues with
ENIG than with HASL or IAg.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of James Mahoney
Sent: Tuesday, August 19, 2008 12:37 PM
To: [log in to unmask]
Subject: Re: [TN] Maximum HASL thickness for SMT of QFN
Yes but I would recommend immersion gold when possible
Thank you,
Jim Mahoney
Quick Turn Flex Circuits, LLC
Applications Project Manager
P# 603-821-6571
F# 603-821-5723
M# 603-305-6250
** This email and all attachments have been scanned prior to being
sent** Confidentiality Notice: This page and any accompanying documents
contain information that is confidential, privileged or exempt from
disclosure and is intended for the exclusive use of the addressee. If
you are not the intended recipient, you are hereby notified that any
disclosure, copying, distribution or use of the contents of this
information in any manner is strictly prohibited.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of James Verrette
Sent: Tuesday, August 19, 2008 1:22 PM
To: [log in to unmask]
Subject: [TN] Maximum HASL thickness for SMT of QFN
What is the maximum SnPb HASL thickness/uniformity that can be tolerated
in the SMT assembly of a .5mm pitch QFN package? Is there anyone else
out there putting .5mm pitch parts on HASL finished boards that is
willing to share their experiences?
Jim Verrette
Senior Electrical Engineer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|