Dexter also markets an in-line system for Teledyne Halco machines. Their 
equipment is based on the same theory as explained below, but it works as the 
Halco works. This allows a consistent copper level as opposed to the batch 
systems where copper builds to a point and then cleaned.

[log in to unmask]


Bob Mesick <[log in to unmask]> Wrote:
| 
| I saw a message over New Years that I don't have any more 
| form someone who
| wanted to remove copper for a solder bath.
| 
| If you heat the bath to just over the eutectic point, I 
| believe its 3 or 4
| deg F over, and let it sit, the copper comes to the top as 
| a copper colored
| scum.  You can just skim it off.  It takes 8-12 hours of 
| sitting.  There is
| still copper in the solder but the concentration is low 
| enough to test OK
| and it solders bright again.
| 
| Some of the solder coating services used to buy or make an 
| extra solderpot
| just to hold the dross and old solder at the eutectic 
| point to purify it.
| 
| Regards,
| 
| Bob Mesick
| 
| Remco Engineering
| Industrial Water and Wastewater Treatment Systems
| San Luis Obispo, California  USA
| 
| **********************************************************
| *****************
| * TechNet mail list is provided as a service by IPC using 
| SmartList v3.05 *
| **********************************************************
| *****************
| * To unsubscribe from this list at any time, send a 
| message to:           *
| * [log in to unmask] with <subject: unsubscribe> and 
| no text.        *
| **********************************************************
| *****************
| * If you are having a problem with the IPC TechNet forum 
| please contact   *
| * Dmitriy Sklyar at 847-509-9700 ext. 311 or email at 
| [log in to unmask]      *
| **********************************************************
| *****************
| 
| 

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2