Both Actually. Some die are attached with flux and others with conductive
epoxy.
>From: Vladimir Igoshev <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>, Vladimir
>Igoshev <[log in to unmask]>
>To: [log in to unmask]
>Subject: Re: [TN] Die Attach
>Date: Sat, 22 Apr 2006 09:00:00 -0400
>
>Hi Scott,
>
>Are soldering or usind conductive epoxy for die attach?
>
>Regards,
>
>Vladimir
>Sent from my Blackberry Wireless
>Vladimir Igoshev, 519-888-7465 ext.5283
>
>
>----- Original Message -----
>From: TechNet <[log in to unmask]>
>To: [log in to unmask] <[log in to unmask]>
>Sent: Sat Apr 22 08:45:06 2006
>Subject: [TN] Die Attach
>
>Got a question for you die attach gurus. We are currently using boards with
>electroless gold finish. We have a supplier that has sent in boards with
>electro-plated gold and we are seeing our die shear's going down. I would
>expect to see some decrease in die shears but we are seeing in some cases
>50% reduction. Any body out there doing both types of gold finishes and if
>so are your parameters and things like flux the same for both?
>
>
>Thanks
>
>
>Scott B. Westheimer
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>
>
>
>---------------------------------------------------------------------
>This transmission (including any attachments) may contain confidential
>information, privileged material (including material protected by the
>solicitor-client or other applicable privileges), or constitute non-public
>information. Any use of this information by anyone other than the intended
>recipient is prohibited. If you have received this transmission in error,
>please immediately reply to the sender and delete this information from
>your system. Use, dissemination, distribution, or reproduction of this
>transmission by unintended recipients is not authorized and may be
>unlawful.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|