Hello there!
I'ld like to get some information regarding the thermal
aging of solder joints, particularly with the following conditions:
1. Solder used:
63/37 and 96/04 (4% silver)
2. Product operating temperature; 187C
What I'm really looking for is the behaviour of solder joint
strength as a function of temperature. If you have any related reports or
literature, please email it to me or link me to the source.
Thanks for your help,
Sincerely,
Reggie Malli
Manager Process Engineering
Glenayre Manufacturing Ltd.
Phone: 604-293-1611
Fax: 604-293-4390
Email: [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|