TECHNET Archives

September 2011

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Eric Christison <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Wed, 14 Sep 2011 10:20:47 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Cedric ORAIN <[log in to unmask]>
Message-ID:
<042601cc72b7$37672530$a6356f90$@[log in to unmask]>
Subject:
From:
Cedric ORAIN <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (123 lines)
You right off-course, "finition" is definitely more French than English !

Thanks to you Eric.

-----Message d'origine-----
De : Eric Christison [mailto:[log in to unmask]] 
Envoyé : mercredi 14 septembre 2011 10:07
À : TechNet E-Mail Forum; Cedric ORAIN
Objet : Re: [TN] Sn100C

"finitions"

Cedric,

You have invented a new word in English, congratulations!

I'm afraid I can't help you but I guess you mean "finishes", in case anyone
else is maybe wondering what your new word is.

Regards,





On 14/09/2011 08:20, Cedric ORAIN wrote:
> Good morning again !
>
>
>
> This is the second subject for which I need your help today. During
previous
> work -when I qualified lead free assembly years ago- several PCB finitions
> was compared. Among the finitions we tested, HAL Sn100C was rejected
because
> of reflow issues using SAC305 solder paste.
>
>
>
> Problems were lack of solderability. I assumed that the reason was because
> of the difference between liquidus of Sn100c in comparaison with SAC305.
We
> didn't make a lot of work to solve that as we head quickly to ENIG and I
> finally rejected Sn100C. until this week when a customer request Sn100C
for
> cost reason.
>
>
>
> So I would appreciate testimony of technetters that use successfully
Sn100C
> as PCB finition with SMD process as well as troubleshooting feedback
> regarding this process.
>
>
>
> Regards,
>
>
>
> Cedric
>
>   <http://www.inovelec-group.com>  www.inovelec-group.com
>
>
>
>
>
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 16.0
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> For additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
> -----------------------------------------------------
> .
>

-- 
Eric Christison
Consumer&  Micro group
Imaging Division

STMicroelectronics (R&D) Ltd
33 Pinkhill
Edinburgh EH12 7BF
United Kingdom

Tel:	+44 (0)131 336 6165
Fax:	+ 44 (0)131 336 6001

The contents of the email are ST confidential.




______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 16.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
For additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2