Eddy wrote:
> Hi technetters,
>
> Is there anyone out there working on "Carbon ,Silver Thru-Hole
> process"?
> We are try the new process.Any guide will be much appreciate.
>
> Thanks,
> Eddy Chen
> EVERGREEN HITECH CONSULTANTS LTD.
> TEL:886-2-27667722 FAX:886-2-27630734
> E-MAIL: [log in to unmask]
> 7th Fl., No. 35, Lane 13, KWAN FU SOUTH ROAD TAIPEI,TAIWAN
> http://www.asiansources.com/evhitech.co
>
>
> -------------------------------------------------------------------------------------------------------------
>
> Eddy,
> Yes,we are.The appliccation:A keyboard with carbon
> contacts,silver/copper conductive paste
> filled vias (plugged) and OSP on solder pads.The circuit is wave
> sodered on the contact side.
> What would you like to know?
> Gaby
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|