We use SERA for solderability evaluation of bare HASL boards, with the V2
pass/fail criteria of the Mil spec P-55110E.
Regards,
Bev Christian
Nortel
613-967-5407
> -----Original Message-----
> From: Wade Oberle [SMTP:[log in to unmask]]
> Sent: Tuesday, January 19, 1999 12:54 PM
> To: [log in to unmask]
> Subject: [TN] SERA
>
> Dear Technetters,
> Does anyone use the SERA technique/equipment for solderability
> testing or evaluation? Dave H at Rockwell seems to be one of the
> experts on this topic. Can Dave or someone else tell me who sells this
> equipment and a phone number and if this equipment is accepted by
> industry?
>
> Regards,
>
> Wade Oberle
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
> section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
> 847-509-9700 ext.312
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|