I just went through this same exercise some weeks back. Most solid test
data that I found supported the premise that in a typical office
environment there will be little to no negative impact on the
solderablity of a "properly" coated HASL board, on at least up to a 2
year period.
Moisture absorption could however be more of a real concern.
Rich K - KEDS
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Black, Paul
Sent: Tuesday, August 09, 2005 2:32 PM
To: [log in to unmask]
Subject: [TN] PCB Storage
Hi All,
I have some bare PC boards that may be built up in the future, but not
in the near future. I would like to put them into storage until needed
(anywhere from 6 months to 2 years). The boards are .062" FR-4 HASL
boards. What would you recommend for protection, assuming that the
storage conditions are typical of an office environment? Would I have to
do anything special to them when they are removed from storage? Any
suggestions would be greatly appreciated.
Thank you,
Paul Black
Manufacturing Engineer
Kronos
E-mail: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|