Phil:
It has been successfully used by several shops. Data Solder Inc, which is a hot air leveling service in Santa Ana has been using it for a couple of years now; they are using tin/copper/cobalt type LF solder.
You can contact Irma Gomez, Data Solder Inc for first hand information at (714) 429 9866 or me at the following #.
Nimal
Nimal Liyanage,Ph.D.
Metallic Resources Inc.
2116 Enterprise Parkway
Twinsburg, OH 44087
330 425 3155
949 697 5826
----- Original Message ----
From: Phil Nutting <[log in to unmask]>
To: [log in to unmask]
Sent: Wednesday, October 24, 2007 9:13:22 AM
Subject: [TN] Lead-free HASL
For years we knew and loved Pb HASL. With the requirements of RoHS HASL
took a back seat. Has L-F HASL had the kinks worked out so it is
becoming a main stream process? If so, who is doing it and what is the
performance of the process? Is it being used for SMT?
Thanks in advance,
Phil Nutting
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|