TECHNET Archives

July 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Shoukai Zhang <[log in to unmask]>
Date:
Wed, 11 Jul 2001 22:27:57 +0100
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Andrew Hoggan <[log in to unmask]>
Subject:
From:
Andrew Hoggan <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="iso-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (56 lines)
Possibly the concern comes through a lack of control in applying immersion
gold compared to other forms of plating. If there is too much gold, then the
intermetallic formed on soldering would potentially interfere with the
solder joint integrity, potentially causing fracture. I couldn't speculate
further without more information on your concern.

Andrew Hoggan
BBA Associates Ltd
www.bba-associates.com

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Shoukai Zhang
Sent: Wednesday, July 11, 2001 10:27
To: [log in to unmask]
Subject: [TN] PCB surface finishes


Dear TechNetters:

As we know that the preferred metal surface finishes are HASL, EN/IG
(Electroless Nickel and Immersion Gold, and OSP etc.

It's reported that EN/IG(also called immersion gold) suface may lead
unreliable solder joint for BGA component,  and suggest do not use
immersion gold for designs that have BGAs.

Please give your advices.

Thanks with best regards,
Zhangshoukai, PE, Huawei Technologies.

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2