When I was at IPC last April, MacDermid had a conveyorized copper treatment
process which had a very small footprint. I talked to Bob Hamilton of
MacDermid who is their technical specialist for this process. You can call
him in the US at (203) 575-5700.
Regards,
Dave Sullivan
Rockwell Collins
J M <[log in to unmask]> on 10/08/98 01:24:47 PM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
to J M <[log in to unmask]>
To: [log in to unmask]
cc:
Subject: [TN] Oxide / Durabond Alternatives
We are in the process of selecting a new line for prelamination, and we
would like to know of other proven alternatives to Oxide/Durabond.
We also would like to have a fully conveyorized system capable of
linking to conveyorized AOI and to Lamination.
Thank you for your help
______________________________________________________
Get Your Private, Free Email at http://www.hotmail.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|