Honoured Messieurs wet chemists,
have to make solderable finish on AlSiC substrates. Got copper plated
samples from manufacturer. We did usual 300 Centigrade blister test, and as
expected, large blisters were created. Now, what suitable finish do you
recommend? Would like to try nickel sputter+electrolytic nickel+gold flash,
but there may be wet chemistry for the adhesion layer instead of sputtering
or thermal spray. There are tin plating methods too, but they seem not to
be for soldering , but rather act as environment protection coatings.
Inge
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|