We are looking at an alternative component replacement for one of our
existing part numbers. The component is a 1206 chip capacitor. The
termination finish on the spec sheets of the existing part is defined as

Base Metallization  -  Silver
Barrier Layer - Nickel
Final Tinned Layer ( 100% Tin)

The replacement part has

Base Metallization - Silver
Barrier Layer - Copper
Final Layer of Solder

The part will go through wave soldering. Is there going to be a
solderability issue?  I have read that the barrier layer's role is to avoid
dissolving into the base mteal and form intermetallics. Is this correct? I
would appreciate if someone would explain the use of different base layers
and their functionality? Silver vs Copper?


thanks


Nasir Hanif
Plexus
[log in to unmask]

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2