TECHNET Archives

August 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Kelly <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Date:
Wed, 11 Aug 2004 16:46:35 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (49 lines)
Hi Dave,
A couple of comments a) shouldn't your gold be soft for wire bonding?.b) if
you have the boards plasma washed in 80 % argon and 20% oxygen you will get
rid of any organic compounds. Regards Steve Kelly

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: Wednesday, August 11, 2004 4:01 PM
To: [log in to unmask]
Subject: [TN] Hard Gold Plating/Contaminate Question


Hi TechNet! Hey, looking for some help (Rudy, Frank, Gerard, plating folks).
Background:  I have a test board which with approximately 80 uinches of
wirebondable hard gold plating that is having gold wirebond process
problems. An XPS (xray photoelectron spectroscopy) analysis of a "good"
versus "bad" test board revealed that the "bad" has significant organic
surface contamination for carbon and oxygen in the form of a hydrocarbon
(lots of C-C and C-H bonds). Now the question: can/will a hydrocarbon
species be codeposited into the gold plating thickness? I understand the
surface process/issues but the codeposit question came up.

Dave Hillman
Rockwell Collins
[log in to unmask]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2