I haven't soldered zinc to a board but we have used cast zinc lugs that get wire soldered to them. We tin them first and I love the thin film it leaves on top of the solder pot.
Charles Caswell
-----Original Message-----
From: David Douthit [mailto:[log in to unmask]]
Sent: Friday, August 30, 2002 2:09 PM
To: [log in to unmask]
Subject: Re: [TN] Zinc casting and solderability
Phil,
Zinc will grow "whiskers" just like tin!
David A. Douthit
Manager
LoCan LLC
Phil Bavaro wrote:
> Here is a question that I do not recall having come across ever before.
>
> A mechanical designer has posed the question of substituting zinc in place
> of a copper as a raw material. This part will be required to be soldered
> down to the circuit card it interfaces with as this is an RF assembly.
>
> Since Zinc alloys are very good for casting definition, is it also possible
> to use Zinc as the base metal.
>
> Or does it require sealing with nickel and then tin plated in order to be
> used for soldering applications?
>
> I realize that some of the new leadfree alloys contain low percentages of
> zinc but this question is oriented towards high contents of zinc in the alloy.
>
> I will keep researching this topic but my first thoughts were that the
> experts on this panel should be able to point me in the right direction at
> least.
>
> Phillip A. Bavaro
> QUALCO/\/\/\/\ Incorporated
> CCA Technical Support
> Engineer, Senior
> [log in to unmask]
> Pager (858) 271-3640
> Tel (858) 658-2542 Voice mail
> Cell (858) 682-6434 (offsite, after hours)
> Fax (858) 658-1584
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|