In IPC specification ANSI/IPC-RB-276, 1992, for "Qualification and Performance Specification
for Rigid Printed Boards" it is specified a copper thickness of 15µm for buried and blind vias
with a min.thickness of 13µm. However this spec. was changed during 1996, IPC-6012, there the
copper thickness for blind vias were increased to an average thickness of 25µm with a min.
thickness of 20µm.
Does anyone know why they changed their specifications?
Is there someone who has any experience of blind and buried vias with thin copper coatings
(15-13µm)?
Thanks in advance for your help
//Markus
Markus Gauffin M.Sc.
Printed Board Assembly Technology
tel: +46 8 719 16 34
fax: +46 8 719 71 99
e-post: [log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]> *
* with <subject: subscribe/unsubscribe> and no text in the body. *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask] *
***************************************************************************
|
|
|