TECHNET Archives

September 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Franklin D Asbell <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 27 Sep 2000 07:13:53 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (58 lines)
Jacob,

Actually IPC 6012 states the opposite, vias may be completely plugged.
If you have access to 6012 look at table 1-1 for plated holes (including
vias).

When plating is not desired in vias the requirement is typically to tent
them with solder mask.

Franklin


"" wrote:

>
>
> Technetter,
>
> 1) Is there any spec that says no solder is allowed in via holes
> (<22mil) especially the HASL boards?
>
> I've encountered a numerous of HASL boards with this problem. Due to
> the solder in via hole, solder lump will start to form at the annular
> ring of the via holes & it causes uneveness solder paste printing as
> well as posibilities of damaging the solder paste stencil. The solder
> lump will only form after the first IR reflow & with the via hole
> facing downward. When it's going for its second round of SMT, the
> problem start to appear, bridging.
>
> 2) Is there any recommended solutions to this problem?
>
> Another input, most of these boards were plugged either from the
> primary or the secondary side. In my case, we'll always mount the
> plugged side first & then followed by the other side.
>
> 3) Is there such a design rule that the process has to go the other
> way round? Meaning, mount on the unplugged side first insteads of the
> plugged side.
>
> Regards,
>
> Jacob Pao (SQE)
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2