TECHNET Archives

May 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 26 May 2006 13:25:31 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Werner Engelmaier <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"; format=flowed
Content-Transfer-Encoding:
7bit
Parts/Attachments:
text/plain (151 lines)
Hi Jeff,
I have suggested that tongue firmly in cheek some time ago.
Werner

-----Original Message-----
From: Jeffrey Bush <[log in to unmask]>
To: [log in to unmask]
Sent: Fri, 26 May 2006 12:49:25 -0400
Subject: Re: [TN] Rohs Weeeeeee board material

    How about a law that says no lead-free assemblies are allowed in the
USA
after June 30 2006.


Jeffrey Bush
Director, Quality Assurance and Technical Support
VERMONT CIRCUITS INCORPORATED
           76 Technology Drive - POB 1890
              Brattleboro, Vermont 05302
                Voice - 802.257.4571 ext 21
                    Fax - 802.257.0011
                       <http://www.vtcircuits.com/>


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Happy Holden
Sent: Friday, May 26, 2006 12:33 PM
To: [log in to unmask]
Subject: Re: [TN] Rohs Weeeeeee board material

Hi,
That's why we tell all our clients now to adjust their board blueprint
MFG
NOTES with the following additional statements:

1. That the finished multilayer must withstand  (A)The LF assembly
process
description including   a. Peak Temp   b. Time at Peak Temp    c Total
time above 250C on heating and cooling    d. Number of Cycles of
a.+b.+c.
    and   (B) If repair and rework is going to be performed and what
those
Time & Temp will be.

2. That the finished multilayer must withstand 3 cycles of a 288C-10
sec.
solder-dip without delamination or hole cracking, measures and checked
in
 (a) Ground-plane area    AND   (b) In the BGA area       before the
board
is shipped.


Happy Holden
Asian Pacific Materials



"Stadem, Richard D." <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
05/26/2006 11:56 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Stadem, Richard D." <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] Rohs Weeeeeee board material






That is the purpose of a thorough process/procedures audit done
periodically to ensure the material received is going to be good.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea, Ioan
Sent: Friday, May 26, 2006 10:50 AM
To: [log in to unmask]
Subject: Re: [TN] Rohs Weeeeeee board material

Hi,

I guess we have a good idea now of the difficulties in specifying and
manufacturing lead-free capable PCBs. The next question that comes to my
mind is how are we going to assess if the PCBs that are well speced are
what we expect?

I mean, the spec can be OK, whether perfect IPC-4010 slash sheets are
developed, or STII is implanted. But the manufacturer might still use
expired prepregs, they can have lamination problems, and so on.

What tests shall a contract manufacturer or OEM with no in-house testing
capability impose, in order to have the confidence that they receive
what they specified?

Thanks,

Ioan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2