Chris;
This is the Holy Grail for all SM, underfill, moulding compounds, etc.
suppliers. Unfortunately, to make epoxies at a reasonable price requires the
use of epichlorohydrin. This reaction will leave free chlorides, in addition
to hydrolyzable chlorides. We do obtain some reasoably "clean" epoxy resins
from Ciba and from Japan. However, these still require additional clean-up for
use in most of our specialty applications.
So to answer your question - besides Ciba and our proprietary japanese source
we have not found any.
Leo Roos
Dexter Electronic Materials
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|