text/plain (75 lines)
Jamie Baumgart wrote about the Aussie board shop using a Direct
Metallisation process - absolutely correct. The company is Lintek and is
located in Canberra, Australia. The principal is Steve Butler, who
developed their process. As far as I know they are still in business using
this process.

Regards,

Wes Smith.


>
>     A gentleman by the name of Gerald White in Mesquite, Texas (just 
>     outside of Dallas) patented a process many years ago using a variation 
>     of sputtering.  He used the term "Mag-ion" plating.  Texas Instruments 
>     had played around with it for several different uses, unfortunately I 
>     left before any really useful information came out of the project. 
>     (This was about 4 years ago.)  
>     
>     I also believe that an Australia PCB shop (Linguard or something like 
>     that) has been producing boards with this process for several years.
>     
>     Regards,
>     Jamie Baumgart  
>
>
>______________________________ Reply Separator
_________________________________
>Subject: Direct metallization
>Author:  [log in to unmask] at smtplink
>Date:    12/27/96 9:33 PM
>
>
>I have heard rumors from a few suppliers around the industry there is a
>research group that is attempting a direct metalization method through a
>plasma sputter  coater. Has anybody heard of such research?
>
>T. Gaylor 
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To unsubscribe from this list at any time, send a message to:           *
>* [log in to unmask] with <subject: unsubscribe> and no text.        *
>***************************************************************************
>* If you are having a problem with the IPC TechNet forum please contact   *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
>***************************************************************************
>
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To unsubscribe from this list at any time, send a message to:           *
>* [log in to unmask] with <subject: unsubscribe> and no text.        *
>***************************************************************************
>* If you are having a problem with the IPC TechNet forum please contact   *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
>***************************************************************************
>
>
>

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2